This article is a comprehensive collection of formulas and numerical solutions, addressing many heat-transfer scenarios encountered in welds. It provides detailed explanations and dimensioned drawings in order to discuss the geometry of weld models, transfer of energy and heat in welds, microstructure evaluation, thermal stress analysis, and fluid flow in the weld pool.

You do not currently have access to this chapter.
Don't already have an account? Register

John Goldak, Mahyar Asadi, Lennart Karlsson, Numerical Aspects of Modeling Welds, Welding Fundamentals and Processes, Vol 6A, ASM Handbook, Edited By T. Lienert, T. Siewert, S. Babu, V. Acoff, ASM International, 2011, p 819–829, https://doi.org/10.31399/asm.hb.v06a.a0005587