Abstract

This article describes the process applications, advantages, and limitations of resistance seam welding. The fundamentals of lap seam welding are also reviewed. The article details the types of seam welds, namely, lap seam welds and mash seam welds, and the processing equipment used for lap seam welding. The primary factors used to determine the selection of electrodes, including alloy type and wheel configuration, are reviewed. The article also describes weld quality and process control procedures.