Flash welding, also called flash butt welding, is a resistance welding process in which a butt joint weld is produced by a flashing action and by the application of pressure. The flash welding process consists of preweld preparation, flashing, upsetting (forging), and postweld heat treatment. This article provides an overview of both flash welding and upset welding and describes the various process and failure origins of flash welding as well as the equipment used. It also explains the characteristics and advantages of solid-state upset welding.
Sign in
ASM members
Member Sign InR. (Bob) Matteson, 2011. "Flash Welding and Upset Welding", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff
Download citation file:
Close
ASM Reference Publications Catalog
The new Fall / Winter 2019-2020 Catalog features more than 200 new and upcoming releases and our popular best-selling titles. Save now with prepublication pricing and set sales.