This article provides a history of electron and laser beam welding, discusses the properties of electrons and photons used for welding, and contrasts electron and laser beam welding. It presents a comparison of the electron and laser beam welding processes. The article also illustrates constant power density boundaries, showing the relationship between the focused beam diameter and the absorbed beam power for approximate regions of keyhole-mode welding, conduction-mode welding, cutting, and drilling.

Abstract

This article introduces the operating principles and modes of operation for high-vacuum (EBW-HV), Medium-vacuum (EBW-MV), and nonvacuum (EBW-NV) electron beam welding. Equipment, process sequence, part preparation, process control, and weld geometry are described for electron beam welding. Advantages are described in terms of welding near heat sensitive components or materials and producing deep penetration or shallow welds with the same equipment.

You do not currently have access to this chapter.
Don't already have an account? Register

High Energy Electron Beam and Laser Beam Welding, Welding Fundamentals and Processes, Vol 6A, ASM Handbook, Edited By T. Lienert, T. Siewert, S. Babu, V. Acoff, ASM International, 2011

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal