Skip to Main Content
ASM Handbook

Casting

Edited by
Srinath Viswanathan
Srinath Viswanathan
Search for other works by this author on:
;
Diran Apelian
Diran Apelian
Search for other works by this author on:
;
Raymond J. Donahue
Raymond J. Donahue
Search for other works by this author on:
;
Babu DasGupta
Babu DasGupta
Search for other works by this author on:
;
Michael Gywn
Michael Gywn
Search for other works by this author on:
;
John L. Jorstad
John L. Jorstad
Search for other works by this author on:
;
Raymond W. Monroe
Raymond W. Monroe
Search for other works by this author on:
;
Mahi Sahoo
Mahi Sahoo
Search for other works by this author on:
;
Thomas E. Prucha
Thomas E. Prucha
Search for other works by this author on:
;
Daniel Twarog
Daniel Twarog
Search for other works by this author on:
ASM International
Volume
15
ISBN electronic:
978-1-62708-187-0
Publication date:
2008
Book Chapter

Eutectic Solidification—An Introduction

By
Sumanth Shankar
Sumanth Shankar
McMaster University
Search for other works by this author on:
Published:
2008
Page range:
307 - 311
Publication history
September 15, 2008

Abstract

This article presents the binary eutectic phase diagram to understand the various structures that evolve in a binary eutectic system during solidification. It describes the various classifications and solidification principles of the eutectic structures. Formation of halos in eutectic microstructures of most alloy systems is also discussed.

You do not currently have access to this content.
Don't already have an account? Register

Sumanth Shankar, 2008. "Eutectic Solidification—An Introduction", Casting, Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal