Abstract

This article describes the applications, advantages, and disadvantages of three centrifugal casting processes as well as the equipment used. The processes include true centrifugal casting (horizontal, vertical, or inclined) semicentrifugal (centrifugal mold) casting, and centrifuge mold (centrifugal die) casting. The article discusses the cooling, inoculation, fluxing, and extraction of casting. It reviews mold heating and coating techniques as well as various molds used for the centrifugal casting processes. The three most common defects observed in centrifugal castings are also discussed. The article concludes with information on the applications of centrifugal force in investment casting and combustion synthesis.

You do not currently have access to this chapter.
Don't already have an account? Register

Sufei Wei, Steve Lampman, 2008. "Centrifugal Casting", Casting, Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal