This article begins with balance equations for mass, momentum, energy, and solute and the necessary boundary conditions for solving problems of interest in casting and solidification. The transport phenomena cover a vast range of length and time scales, from atomic dimensions up to macroscopic casting size and from nanoseconds for interface attachment kinetics to hours for casting solidification. The article describes how to determine which phenomena are most important at the particular length and time scale for the problem. It concludes with several examples of the application of transport phenomena in solidification, focusing in particular on microstructure formation.

You do not currently have access to this chapter.
Don't already have an account? Register

Jonathan A. Dantzig, 2008. "Transport Phenomena During Solidification", Casting, Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal