Abstract

Electroslag remelting (ESR) is commonly used to produce the highest levels of quality in plate steels, particularly in thick plates. This article provides an overview of the ESR and discusses the major components and operations of the ESR furnaces. It describes the principles of ingot solidification and various defects of remelted ingot such as tree ring patterns, freckles, and white spots. The article explains several variations of ESR such as pressure electroslag remelting, remelting under reduced pressure, and electroslag rapid remelting. It examines the features of steel ESR and superalloy ESR.

You do not currently have access to this chapter.
Don't already have an account? Register

2008. "Electroslag Remelting", Casting, Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal