Casting
Design Problems Involving Unequal Sections[1]
-
Published:2008
Abstract
This article addresses the problems of designing isolated heavy sections that are functionally essential. It describes the two most efficient solutions to these problems over which the designer has control: providing flow and feed paths and reducing the mass of the isolated sections. The article concludes with a discussion on designs that reduce the mass of a remote section.
Sign in
ASM members
Member Sign InDesign Problems Involving Unequal Sections, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, https://doi.org/10.31399/asm.hb.v15.a0009023