This article discusses various molten-metal treatments, namely fluxing, degassing, and molten-metal filtration. It focuses on various molten-metal handling systems for transporting, holding, or delivering molten metal to the mold/die system. These include launders, tundishes, holding furnaces or transport crucibles, molten-metal transfer pumps, teeming ladles, and dosing and pouring furnaces.