Abstract

Nickel-base alloy castings are widely used in corrosive-media and high-temperature applications. This article begins with a discussion on the compositions of corrosion-resistant nickel-base casting alloys and heat-resistant nickel-base casting alloys. It describes the effects of aluminum and titanium on the structure and properties of nickel-base alloys. The article provides information on the melting, foundry, and pouring practices for nickel-base alloys. It describes the welding and heat treatment of the nickel-base casting alloys. The article concludes with information on the numerous applications of cast heat-resistant nickel-base alloys.

You do not currently have access to this chapter.
Don't already have an account? Register

Selçuk Kuyucak, Nickel and Nickel Alloy Castings, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 1119–1127, https://doi.org/10.31399/asm.hb.v15.a0005336

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal