Vacuum induction melting (VIM) is often done as the primary melting operation followed by secondary melting (remelting) operations. This article presents the process description of VIM and illustrates potential processing routes for products, which are cast from VIM ingots or electrodes. It describes the VIM refinement process, which includes removal of trace elements, nitrogen and hydrogen degassing, and deoxidation. The article concludes with information on production of nonferrous materials by VIM.

You do not currently have access to this chapter.
Don't already have an account? Register

Vacuum Induction Melting, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 116–123, https://doi.org/10.31399/asm.hb.v15.a0005200

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal