In terms of component design, casting offers a great amount of flexibility. This article discusses the parameters that can drive the geometry of casting design from a process standpoint. It provides information on the design of junctions and addresses considerations of secondary operations in design. The article describes the factors that control casting tolerances and provides specific tips for designing castings with uniform wall thickness and unequal sections, designing thin sections, designing for economical coring, designing for functional packaging, and core design principles. The choice of whether a component is best manufactured as welded, assembled, fabricated, forged, machined, or cast is based on the component geometry, production costs, and requirements in application. The article addresses these issues and provides a framework for analyzing all manners of manufacturing as possible conversion candidates. It concludes with a discussion on different metalcasting design projects.

You do not currently have access to this chapter.
Don't already have an account? Register

Michael Gwyn, Casting Design and Geometry, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, https://doi.org/10.31399/asm.hb.v15.a0009020

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal