Skip to Main Content
Skip Nav Destination

Abstract

This article discusses the requirements that are typically considered in designing a steel casting. It describes the materials selection that forms a part of process of meeting the design criteria. The article provides information on material selection guide for five major design applications. It examines the attributes that are specific to the manufacturing of steel castings. The article concludes with information on various nondestructive examination methods for ensuring manufacturing quality and part performance in steel castings.

You do not currently have access to this chapter.
Don't already have an account? Register
Close Modal

or Create an Account

Close Modal
Close Modal