A gating system is the conduit network through which liquid metal enters a mold and flows to fill the mold cavity, where the metal can then solidify to form the desired casting shape. This article discusses various desirable design considerations for the gating system. Proper design of an optimized gating system will be made easier by the application of several fundamental principles of fluid flow. The article illustrates the Bernoulli's theorem, the law of continuity, and the effect of momentum. Most casting alloys are subject to the presence of particles that can deleteriously affect the physical properties and appearance...