Abstract

This article discusses the melting and poring practices, heat treatment, and applications of different types of high-alloy graphitic iron, namely, high-silicon gray irons, high-silicon ductile irons, nickel-alloyed austenitic irons, austenitic gray irons, austenitic ductile irons, and aluminum-alloyed irons.

You do not currently have access to this chapter.
Don't already have an account? Register

Richard B. Gundlach, High-Alloy Graphitic Irons, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 904–908, https://doi.org/10.31399/asm.hb.v15.a0005328