This article reviews the failure analysis process with specific reference to the considerations that should be addressed when a casting has failed. It describes the failure analysis methodology for three failed cast components: an aluminum bracket, a bronze suction roll, and a steel automotive spindle. The article discusses failure analysis investigation by obtaining casting background information, planning the evaluation and selecting the appropriate casting for analysis, conducting a preliminary examination, conducting the proper material evaluations, and thoroughly evaluating the test data. It concludes with information on case studies that show how the methodology is adapted for differing materials, failure mechanisms, and failure circumstances.

You do not currently have access to this chapter.
Don't already have an account? Register

Craig Brown, Casting Failure Analysis Techniques and Case Studies, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 1183–1191, https://doi.org/10.31399/asm.hb.v15.a0005343

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal