This article reviews the history and methods of copper alloy continuous casting. The methods include vertical continuous casting and horizontal continuous casting. The article discusses the upcasting methods used in vertical continuous casting and strip casting used in horizontal continuous casting. The upcasting methods include Outokumpu upcasting method, Rautomead upwards vertical casting, and pressure upcasting. The article also describes the methods and processes of wheel casting and Ohno continuous casting.

You do not currently have access to this chapter.
Don't already have an account? Register

Derek E. Tyler, Richard P. Vierod, Copper Continuous Casting, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 1019–1025, https://doi.org/10.31399/asm.hb.v15.a0005288

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal