Vertical centrifugal casting machines, installed below the ground level for maximum operator safety, are used for producing bushings and castings that are relatively large in diameter and short in length. This article discusses the mold design for different types of sand molds and permanent molds and their production considerations. It describes the speed of rotation, mold speeds curves, and pouring techniques that are considered in the operation of vertical centrifugal casting machines.

You do not currently have access to this chapter.
Don't already have an account? Register

Y.V. Murty, Vertical Centrifugal Casting, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 680–686, https://doi.org/10.31399/asm.hb.v15.a0005259

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal