Horizontal centrifugal casting is used to cast parts having an axis of revolution. This article discusses the operations of various horizontal casting machines, such as flanged shaft machine, horizontal roller-type machine, and double-face plate machine. It describes the types of molds, such as expendable molds and permanent molds, used for centrifugal casting. The article also discusses the steps in casting process, namely, pouring, solidification, and babbitting. It provides information on the applications of the horizontal centrifugal casting.

You do not currently have access to this chapter.
Don't already have an account? Register

Y.V. Murty, Horizontal Centrifugal Casting, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 674–679, https://doi.org/10.31399/asm.hb.v15.a0005258

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal