Spray casting, also known as spray forming, is a niche casting process for the manufacture of preforms. This article lists commercial examples of alloys manufactured by spray casting and provides sequential steps of the spray casting process. Gas atomization is a chaotic, stochastic process that always produces a wide range of droplet diameters. The article schematically illustrates typical log-normal droplet diameter probability density distribution on a mass or volume basis obtained by gas atomization. It also illustrates the changes in solid fraction during the spray casting process as a function of axial distance from the point of droplet atomization. The article concludes with a section on occurrence of macrosegregation and coarsening in spray cast preforms.

You do not currently have access to this chapter.
Don't already have an account? Register

P.S. Grant, Spray Casting, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 382–385, https://doi.org/10.31399/asm.hb.v15.a0005225

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal