Semisolid metal (SSM) processing is a special die casting process, where partially solidified metal slurry is injected into a die cavity to form die cast components. This article discusses the flow behavior of SSM slurry with emphasis on viscosity, rheological behavior, and yield strength. It illustrates microstructural formation of semisolids, under forced convection. The article concludes with an illustration that compares two SSM processes, namely, thixocasting and rheocasting.

You do not currently have access to this chapter.
Don't already have an account? Register

Qingyue Pan, Diran Apelian, Semisolid Metal Processing, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 379–381, https://doi.org/10.31399/asm.hb.v15.a0005224

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal