Casting
Vacuum High-Pressure Die Casting
-
Published:2008
Abstract
Vacuum high-pressure die casting uses a vacuum pump to evacuate the air and gases from the die casting die cavity and metal delivery system before and during the injection of molten metal. This article describes the conventional die casting, vacuum die casting, and high-pressure die casting processes.
Sign in
ASM members
Member Sign InWilliam A. Butler, Vacuum High-Pressure Die Casting, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 732–733, https://doi.org/10.31399/asm.hb.v15.a0005276
Download citation file: