This article illustrates various rheocasting processes. These include new rheocasting, semisolid rheocasting, subliquidus casting, rheo-diecasting, swirled enthalpy equilibration device process, slurry-on-demand process, and continuous rheoconversion processes.

You do not currently have access to this chapter.
Don't already have an account? Register

Q.Y. Pan, Diran Apelian, John Jorstad, Rheocasting, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 773–776, https://doi.org/10.31399/asm.hb.v15.a0005274