Abstract
In order to model macrosegregation, one must consider convection and the partitioning of the segregating elements at the dendritic length scale. This article describes microsegregation with diffusion in the solid. It presents a continuum model of macrosegregation and illustrates the simulation of macrosegregation and microsegregation.
Sign in
ASM members
Member Sign InD.R. Poirier, J.C. Heinrich, Modeling of Microsegregation and Macrosegregation, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 445–448, https://doi.org/10.31399/asm.hb.v15.a0005237