The vacuum arc remelting (VAR) process is widely used to improve the cleanliness and refine the structure of standard air melted or vacuum induction melted (VIM) ingots and also used in the triplex production of superalloys. This article illustrates the VAR process and the capabilities and variables of the VAR process. It also presents a discussion on the melt solidification, resulting structure, and ingot defects. The article concludes with a discussion on VAR process of superalloy, and titanium and titanium alloy.

You do not currently have access to this chapter.
Don't already have an account? Register

Vacuum Arc Remelting, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 132–138, https://doi.org/10.31399/asm.hb.v15.a0005202

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal