Gas porosity is a major factor in the quality and reliability of castings. The major cause of gas porosity in castings is the evolution of dissolved gases from melting and dross or slag containing gas porosity. Degassing is the process of removing these gases. This article describes the methods of degassing aluminum, magnesium, and copper alloys. It provides information on sources of hydrogen in aluminum and gases in copper.

You do not currently have access to this chapter.
Don't already have an account? Register

David V. Neff, Degassing, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 185–193, https://doi.org/10.31399/asm.hb.v15.a0005353