This article discusses the categories and subcategories of shape casting processes. These include single-use processes, such as sand, plaster, ceramic, and graphite molding; essentially unpressurized multiuse processes, such as permanent mold; and high-pressure metal mold methods, such as die casting, squeeze casting, and semisolid processing. The article contains tables that compare some of the typical capabilities of shape casting processes.

You do not currently have access to this chapter.
Don't already have an account? Register

J.L. Jorstad, Shape Casting Processes—An Introduction, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 485–487, https://doi.org/10.31399/asm.hb.v15.a0005187