The cold chamber die casting process is used with higher-melting-point alloys such as aluminum and magnesium. This article discusses the components design of the cold chamber high-pressure die casting machine. It reviews the process parameters of the cold chamber die casting. The parameters include shot profile, intensification phase, and component size.

You do not currently have access to this chapter.
Don't already have an account? Register

Robert J. McInerney, II, Cold Chamber Die Casting, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 724–726, https://doi.org/10.31399/asm.hb.v15.a0005268