This article provides a comprehensive discussion on die casting alloy types and casting processes used in high-pressure die casting. It presents the advantages and disadvantages of high-pressure die casting and describes the product design for the process. The article concludes with information on metal injection process of high-pressure die casting.

Abstract

This article describes the melting process of casting metals used in hot chamber die casting. It discusses the design and capabilities of injection components, such as gooseneck, plunger, and cylinder. The article reviews the distinctions between hot and cold chamber processes. Gate and runner design and temperature control for die casting are discussed. The article explains the ejection and post-processing techniques used for the hot chamber die casting. The techniques include robotics operation, recycling, and fluxing.

You do not currently have access to this chapter.
Don't already have an account? Register

High-Pressure Die Casting, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal