Abstract

This article discusses the effects of parameters on corrosivity and explains why it is critical to examine the parameter interactions prior to capturing the synergistic effects of the parameters on corrosion. It examines the methods of internal corrosion prediction for multiphase pipelines. The article reviews methodologies to perform internal corrosion direct assessment for pipelines. Real-time monitoring techniques for assessing actual corrosion at critical locations are discussed. The article also presents the case studies for multi-technique electrochemical corrosion monitoring.