Abstract

Several factors contribute to marine-atmospheric corrosion with the local environment being the single most important factor. Therefore, assessing a local environment, which is essential to reduce the gross expenditure, is assisted by modeling of the local environment and by a set of corrosion standards proposed by the International Standards Organization (ISO). This article focuses on the important variables associated with atmospheric corrosion in marine atmospheres, namely, moisture, temperature, winds, airborne contaminants, alloy content, location, and biological organisms along with their corresponding assessing methods. It also examines the ISO CORRAG program for modeling the corrosion rate of atmospheric corrosion that is represented as equations modeling.

You do not currently have access to this chapter.
Don't already have an account? Register

Richard B. Griffin, 2006. "Corrosion in Marine Atmospheres", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal