Abstract

This article focuses on the microbiologically influenced corrosion (MIC) of military assets. It discusses the mechanisms for the MIC in hydrocarbon fuels and atmospheric, immersion, and buried environments with specific examples. The article describes the behavior of metals and alloys, namely, copper alloy, nickel alloy, titanium and titanium alloys, aluminum alloys, stainless steels, and carbon steel in immersion environments.