This article focuses on the corrosion and deterioration of components on recreational and small workboats. It discusses the materials selection and corrosion control for the components. These components include hulls, fittings, fasteners, metal deck gear, winches, backing plates, lifeline supports, inboard engines, cooling systems, propulsion systems, electrical and electronic systems, plumbing systems, masts, spars, and rigging.