This article provides an overview of the principle forms of corrosion that can occur on automotive aluminum components and offers general guidelines on how best to avoid these situations. It discusses the most common forms of aluminum corrosion such as stress-induced corrosion, cosmetic corrosion, crevice corrosion, and galvanic corrosion.