Batteries and fuel cells are popular forms of portable electrical energy sources. This article discusses the operation and corrosion problems inherent in batteries and fuel cells. Batteries are classified into two groups: primary or nonrechargeable batteries and secondary or rechargeable batteries. Fuel cells are classified into five types: phosphoric acid fuel cell (PAFC), solid polymer electrolyte fuel cell, alkaline electrolyte fuel cell, molten carbonate fuel cell (MCFC), and solid oxide fuel cell. The article presents reactions that occur during charging and discharging of lead-acid batteries, PAFC, and MCFC.

You do not currently have access to this chapter.
Don't already have an account? Register

Chester M. Dacres, 2006. "Corrosion in Portable Energy Sources", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.