This article addresses the long-term corrosion behavior of high-level waste (HLW) container materials, more specifically of the outer shell of the containers. It discusses time, environmental, and materials considerations for the emplacement of HLW in geological repositories. Environmental corrosion resistance of materials planned for reducing repositories is also discussed. The article reviews the design and characterization of nuclear waste repository with an oxidizing environment surrounding the waste package.
Sign in
ASM members
Member Sign InRaúl B. Rebak, R. Daniel McCright, Corrosion of Containment Materials for Radioactive-Waste Isolation, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 421–437, https://doi.org/10.31399/asm.hb.v13c.a0004149
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.