This article provides a historical review of corrosion problems in military electronic equipment. It describes the importance of design for corrosion control of an electronic black box used to contain electrical equipment that provides various functions. The article illustrates corrosion control aspects, such as the position of printed circuit boards (PCBs) and proper location of connectors for insertion of the PCBs. It discusses various materials and alloys considered for connectors, PCB contacts, and circuits. The article concludes with a discussion on the effects of contaminants on the electronic black box.

You do not currently have access to this chapter.
Don't already have an account? Register

Joseph T. Menke, Corrosion of Electronic Equipment in Military Environments, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 205–210, https://doi.org/10.31399/asm.hb.v13c.a0004129

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal