Corrosion in Workboats and Recreational Boats
-
Published:2006
Abstract
This article focuses on the corrosion and deterioration of components on recreational and small workboats. It discusses the materials selection and corrosion control for the components. These components include hulls, fittings, fasteners, metal deck gear, winches, backing plates, lifeline supports, inboard engines, cooling systems, propulsion systems, electrical and electronic systems, plumbing systems, masts, spars, and rigging.
Sign in
ASM members
Member Sign InEverett E. Collier, Corrosion in Workboats and Recreational Boats, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 265–278, https://doi.org/10.31399/asm.hb.v13c.a0004139
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.