High-Temperature Corrosion in Waste-to-Energy Boilers
-
Published:2006
Publication history
September 29, 2006
Abstract
This article describes the corrosion modes in a waste-to-energy boiler. It discusses the corrosion protection and alloy performance with an emphasis on two main areas of the boiler: furnace water walls and super heaters.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
George Y. Lai, High-Temperature Corrosion in Waste-to-Energy Boilers, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 482–485, https://doi.org/10.31399/asm.hb.v13c.a0004157
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.