This article focuses on the various coatings used on Department of Defense (DoD) systems. The coatings include electroplated coatings; conversion coatings; supplemental oils, waxes, lubricants; organic paint coatings; and other finishes such as vacuum deposits, mechanical plating, thermal spray coatings, and hot-dip coatings. The article also tabulates test requirements and time to failure of the coatings.