Abstract
This article reviews the understanding of corrosion interactions between alloys in complex geometries and in applications where there are significant cyclic stresses and potential for wear and fretting motion. These alloys include iron-base, titanium-base, and cobalt-base alloys. The article discusses the surface characteristics and electrochemical behavior of metallic biomaterials. It summaries the clinical context for mechanically assisted corrosion and describes mechanically assisted crevice corrosion. There have been several tests developed to investigate aspects of mechanically assisted corrosion. The article also explains the scratch test and the in vitro fretting corrosion test.
Sign in
ASM members
Member Sign InJeremy L. Gilbert, Mechanically Assisted Corrosion of Metallic Biomaterials, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 826–836, https://doi.org/10.31399/asm.hb.v13c.a0004206
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.