Abstract

This article describes the eight chemical cleaning methods, namely, circulation, fill and soak, cascade, foam, vapor-phase organic, steam-injected, on-line chemical, and mechanical cleaning. It presents information on deposit types, solvents used to remove them, and construction material incompatibilities in a table. The article summarizes the uses of chemical cleaning solutions, including hydrochloric acid, phosphoric acid, and sulfamic acid, as well as the additives used to neutralize their impact on corrosion. It discusses the chemical cleaning procedures, including selection of cleaning method and solvent, documentation of cleaning, and corrosion monitoring in chemical cleaning.

You do not currently have access to this chapter.
Don't already have an account? Register

Bert Moniz, Jack W. Horvath, Chemical Cleaning and Cleaning-Related Corrosion of Process Equipment, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 323–330, https://doi.org/10.31399/asm.hb.v13c.a0004143

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal