Abstract

This article reviews corrosion problems in the U.S. Department of Defense (DoD) and discusses management and maintenance aspects of the practices that address the cost and readiness. It describes the plans to institute corrosion prevention and control strategies under DoD directives in engineering design, material selection, and fabrication processes for new acquisitions. The article also presents long-term strategy to reduce the cost of corrosion control.

Abstract

This article provides a perspective on United States (U.S.) Department of Defense (DOD) specifications, standards, handbooks, and related documents, as well as their role in corrosion prevention and control activities in the U.S. military.

Abstract

The major benefit of the implementation of the corrosion-control technologies at Army installations is the extension of the service life of buildings and other structures. This article reviews the exposure of military facilities and equipment to a wide variety of environmental conditions, including soils, waters, or atmospheres of varying corrosivity. It presents the case studies illustrating typical examples of the types of corrosion problems found on military installations. The article describes the various corrosion-control technologies used in military facilities. These include protective coatings and linings, cathodic protection, advanced materials selection and design, water treatment, equipment inspection and monitoring, and below-grade moisture mitigation.

You do not currently have access to this chapter.
Don't already have an account? Register

2006. "Corrosion in Military Environments", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.