This article discusses the corrosion of chromium electrodeposits and the ways for optimizing corrosion resistance. It describes processing steps and conditions for hard chromium plating. The steps include pretreatment, electroplating, and posttreatment. The article also provides information on duplex coatings and applications of chromium electrodeposits.