Abstract

This article contains a galvanic series chart that shows the electrochemical voltage ranges of metals and alloys in flowing seawater. Dark boxes in the chart indicate the active behavior of active-passive alloys.

You do not currently have access to this chapter.
Don't already have an account? Register

2005. "Galvanic Series of Metals and Alloys in Seawater", Corrosion: Materials, Stephen D. Cramer, Bernard S. Covino, Jr.