Corrosion is often thought of as rusting, the process of deterioration undergone by a metal when it is exposed to air or water. This article provides the fundamentals of joints corrosion and primarily addresses the various forms of corrosion observed in brazed and soldered joints and their causes. It describes the role of proper brazing procedures in controlling corrosion. The article concludes with information on the corrosion resistance of various brazing alloy systems.