This article provides a detailed discussion on the most commonly employed tests and specific examples of the use of these tests in evaluating the corrosion resistance of powder metallurgy (P/M) stainless steels. It describes the influence of various processing parameters on the corrosion resistance of P/M stainless steels. The approaches used to improve the corrosion resistance of sintered stainless steels are discussed briefly. The article also presents a discussion on the manufacturing and corrosion characteristics of P/M superalloys.