Introduction to Environmental Performance of Nonmetallic Materials
-
Published:2005
Abstract
This article provides an overview of environmental performance of the most commonly used nonmetallic materials. The materials include elastomers, plastics, thermosetting resins, resin-matrix composites, organic coatings, concrete, refractories, and ceramics. The article also provides information on the applications and uses of these materials.
Sign in
ASM members
Member Sign InDavid C. Silverman, Introduction to Environmental Performance of Nonmetallic Materials, Corrosion: Materials, Vol 13B, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2005, p 545–546, https://doi.org/10.31399/asm.hb.v13b.a0003840