This article begins with the discussion on the background of metal-matrix composites (MMC) and moves into a broad description of the general parameters affecting the corrosion of MMC. It discusses the primary sources of MMC corrosion that include galvanic corrosion between MMC constituents, chemical degradation of interphases and reinforcements, microstructure-influenced corrosion, and processing-induced corrosion. The article elaborates on the corrosion behavior of specific aluminum, magnesium, titanium, copper, stainless steel, lead, depleted uranium, and zinc MMCs systems. It concludes with a description on the corrosion control of MMCs using protective coatings and inhibitors.

You do not currently have access to this chapter.
Don't already have an account? Register

L.H. Hihara, Corrosion of Metal-Matrix Composites, Corrosion: Materials, Vol 13B, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2005, p 526–542, https://doi.org/10.31399/asm.hb.v13b.a0003839

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal